Caution
① If necessary, dry at 300~350°C (572~662°F ) for 60 minutes before use.
② Excessive flux spraying height will damage the bead's appearance, such as a fork mark, so be cautious.
Purpose
① LPG tanks
② Boiler(Fin tube)
Attribute
① Easy to remove slag
② High speed welding
③ Density : 1.0g/cm3
Caution
① If necessary, dry at 300~350°C (572~662°F ) for 60 minutes before use.
② Excessive flux spraying height will damage the bead's appearance, such as a fork mark, so be cautious.
Purpose
① LPG tanks
② Boiler(Fin tube)
Attribute
① Easy to remove slag
② High speed welding
③ Density : 1.0g/cm3
Caution
① If necessary, dry at 300~350°C (572~662°F ) for 60 minutes before use.
② Excessive flux spraying height will damage the bead's appearance, such as a fork mark, so be cautious.
③ When restraint stress is high or welding a thick plate, preheat according to rules.
Purpose
① Heat resistant steels
② Fin-tube
Attribute
① Easy to remove slag
② High speed welding
③ Density : 1.0g/cm3
Caution
① If necessary, dry at 300~350°C (572~662°F ) for 60 minutes before use.
② Excessive flux spraying height will damage the bead's appearance, such as a fork mark, so be cautious.
Purpose
① Heat resistant steels
② Fin-tube
Attribute
① Easy to remove slag
② High speed welding
③ Density : 1.0g/cm3