Caution
① Dry at 300~350℃(572~662℉) for 60 minutes before use.
② In case of multi-layer welding of the thick plate, to prevent cracks, low current and low speed welding should be performed on the lower layer.
③ If weld heat input is managed below 30KJ/cm, a better impact toughness can be achieved.
④ When restraint stress is high or welding a thick plate, preheat according to rules.
Purpose
① LPG tanks
② Spiral Pipes
③ Agricultural implements
Attribute
① Easy to remove slag
② High speed welding
③ Horizontal and flat fillet welding
④ Density : 1.0g/cm3