Caution
① Dry at 300~350°C (572~662°F ) for 60 minutes before use.
② Excessive flux spraying height will damage the bead's appearance, so be cautious.
③ When restraint stress is high or welding a thick plate, preheat according to rules.
Purpose
① Offshore
② Pressure vessels
③ Pipeline
Attribute
① Low hydrogen content
② Tandem, multi-electrode applicable
③ Good impact value at low temperature after heat treatment
④ Density : 1.2g/cm3
Caution
① Dry at 300~350°C (572~662°F ) for 60 minutes before use.
② Excessive flux spraying height will damage the bead's appearance, so be cautious.
③ When restraint stress is high or welding a thick plate, preheat according to rules.
Purpose
① Offshore
② Pressure vessels
③ Pipeline
Attribute
① Low hydrogen content
② Tandem, multi-electrode applicable
③ Good impact value at low temperature after heat treatment
④ Density : 1.2g/cm3
Caution
① Dry at 300~350°C (572~662°F ) for 60 minutes before use.
② Excessive flux spraying height will damage the bead's appearance, so be cautious.
③ When restraint stress is high or welding a thick plate, preheat according to rules.
Purpose
① Offshore
② Pressure vessels
③ Pipeline
Attribute
① Low hydrogen content
② Tandem, multi-electrode applicable
③ Good impact value at low temperature after heat treatment
④ Density : 1.2g/cm3