Caution
① Dry at 300~350°C (572~662°F ) for 60 minutes before use.
② In case of multi-layer welding of the thick plate, to prevent cracks, low current and low speed welding should be performed on the lower layer.
③ If weld heat input is managed below 30KJ/cm, a better impact toughness can be achieved.
④ When restraint stress is high or welding a thick plate, preheat according to rules.
Purpose
① Shipbuilding
Attribute
① Both side single-layer welding
② Low consumption of flux
③ Density : 1.2g/cm3