Caution
① Dry at 300~350°C (572~662°F ) for 60 minutes before use.
② Excessive flux spraying height will damage the bead's appearance, so be cautious.
③ When restraint stress is high or welding a thick plate, preheat according to rules.
Purpose
① LPG tanks
② General fabrication
③ Structural fabrication
Attribute
① Easy to remove slag
② High speed welding
③ Horizontal and flat fillet welding
④ Density : 1.2g/cm3
Caution
① Dry the flux at 300~350°C (572~662°F ) for 60 minutes before use.
② Excessive flux spraying height will damage the bead's appearance, so be cautious.
③ When restraint stress is high or welding a thick plate, preheat according to rules.
Purpose
① LPG tanks
② General fabrication
③ Structural fabrication
Attribute
① Easy to remove slag
② High speed welding
③ Horizontal and flat fillet welding
④ Density : 1.2g/cm3