Caution
① Dry at 300~350°C (572~662°F ) for 60 minutes before use.
② Insufficient amount of flux spray may result in poor bead appearance as well as welding defects.
③ Add new flux periodically, since re-usage of the flux cause welding defects and bad bead appearance.
④ When restraint stress is high or welding a thick plate, preheat according to rules.
Purpose
① Shipbuilding (one-side welding)
Attribute
① High deposition rate with high input use
② Suitable for one side welding of TMCP steel
③ Density : 1.3g/cm3